Abstract

In this paper, the 3.5 vol.%TiB reinforced TC4 (Ti6Al4V) matrix composites were successfully fabricated using a mechanical ball milling and spark plasma sintering. The sintering temperature, sintering pressure and holding time were 700 °C~1100 °C, 40 MPa and 5 min, respectively. The 3.5 vol.% TiB/ TC4 matrix composites. The relative density of 3.5 vol.% TiB/TC4 composites increases with the increase of sintering temperature, and reaches saturation when the sintering temperature is 900 °C. The size of α-Lamellae increases from 1.47 μm to 2.44 μm with the increase of sintering temperature. The aspect ratio of TiB whiskers first increase and then decreases along with the solution time extending.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.