Lead free 0.95[(K0.5Na0.5)1−xAgxNbO3]–0.05LiSbO3 (KNAN–LS) ceramics with x = 0, 0.02, 0.04, 0.06 and 0.08 have been synthesized by conventional solid state reaction route (CSSR). X-ray diffraction (XRD) analysis confirmed the transformation of mixed structure to pure tetragonal structure with the increase in Ag content in KNN–LS ceramics. The Curie temperature (Tc) of the ceramics decreased from 385.5 °C to 331 °C with the increase in silver (Ag) content. The poling temperature was optimized for better piezoelectric properties. The KNAN–LS ceramics with x = 0.06 showed better piezoelectric and ferroelectric properties (d33 = 227 pC/N, kp = 42.5%, Tc = 368 °C and Pr = 21.9 μC/cm2).

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.