1. Steel Kh20N20 alloyed with up to 5% Si is not embrittled on tempering up to 10 h. With 6% Si the steel is embrittled in 1 h. 2. The embrittlement of steel Kh20N20 with 6% Si and steel Kh20N20 with more than 4% Si on prolonged tempering (over 100 h) is evidently due to the precipitation of an intermetallic phase enriched in silicon.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.