Abstract

The oxidation of four Ni-xSi-6Al alloys (x = 0, 2,4 and 6 at.%) has been studied at 1273 K under 0.1 MPa O-2. Silicon exerts the third-element effect by reducing the critical Al content needed for the transition from its internal to its external oxidation with respect to Ni-Al alloys. This result is interpreted by extending to ternary alloys Wagner's criterion for the same transition in binary alloys. (c) 2005 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.