In this study, the W-Si-C multi-phase composites were fabricated by an arc melting method. With addition of SiC, the grain size of W is obviously reduced, and the small angle misorientation becomes dominate, which is beneficial for the improvement of deformability. The effects of SiC additions (from 0.5 to 3wt%) on the microstructure and mechanical properties are mainly investigated. With 1 wt% SiC addition, the flexural strength reaches the highest value. The self-generation of W5Si3 may enhance the strength and ductility, but too much W5Si3 exists as brittle BP (Brittle to Plastic) microstructure. The highest flexural strength is obtained at approximately 1 vol% W5Si3.