Abstract

We examined the effects of Si and Al content of Fe-Si-Al alloy powders with respect to the temperature dependence of core loss in order to find an optimum composition that achieves both negative temperature dependence of core loss and good permeability. By reducing the Si content from the 9.6 mass% of conventional Sendust alloy composition to 7.9-8.9 mass%, the temperature dependence of core loss became negative and maintained the high permeability of the Sendust powder core. The optimum composition was 8.8 mass% Si and 6.0 mass% Al, yielding a core loss value of 240 kW/m/sup 3/ at 373 K, about half that of the conventional Sendust powder core.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.