Abstract
The effects of Nd-Fe-B magnet scrap size on extraction behavior were investigated by liquid metal extraction using molten Mg. The magnet scraps with Mg were placed into a stainless steel crucible and then heated to 1,073K for 10 to 50min. The amount of extracted Nd after liquid metal extraction process was increased with an increasing with holding time and scrap size, and the maximum contents of Nd in Mg were observed to be about 24.2 wt.% in the conditions of the 5mm sized scrap heated for 50min. It was revealed that Nd oxides existing in the magnet scraps prevent the dissolution of Nd into Mg.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.