Abstract
Grain refinement is one of the effective methods to improve the yield strength and toughness of Al-Cu alloys. The effects of Sc addition (0.2%, 0.4%, 0.6%, 0.8% and 1.0 wt%) on the microstructural evolution and mechanical properties of as-cast Al-5%Cu alloys were studied. The as-cast samples were characterized by optical microscope (OM), transmission electron microscopy (TEM), scanning electron microscope (SEM) and electron probe microanalysis (EPMA). The results revealed the primary α-Al occurred to obvious change from developed dendrites to fine equiaxed grains with the increasing Sc content in Al-5%Cu alloy. When the addition concentration of Sc reaches 0.8%, the developed α-Al dendrites were significantly refined and the average size of α-Al decreased from 218.3 μm to 29.6 μm. Moreover, the morphology and size of θ-Al2Cu phases of Al-5%Cu alloy caused noticeable changes with the increase of Sc concentration. Mechanical properties test illustrated that the ultimate tensile strength (UTS), yield strength (YS) and elongation (El) increased by 61.59%, 66.82% and 57.20%, respectively, which could be attributed to microstructure refinement and fine Al3Sc particle precipitate.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.