Abstract

Mg<sub>2</sub>(Si,Sn)-based thermoelectric materials, which are environmentally friendly and low-cost, have great development potential in a moderate temperature range. Electronic transport properties of Mg<sub>2</sub>Si<sub>1-<i>x</i></sub>Sn<sub><i>x</i></sub> alloys can be optimized by doping elements. Doping is still one of the most effective methods of optimizing electronic transport performance, such as carrier concentration, mobility, and effective mass. The most effective doping elements are Sb and Bi. Much attention has been paid to the influence of element type and doping content. Different substitution sites will also greatly affect the electronic transport parameters. In this work, the defect formation energy value of Mg<sub>2</sub>Si<sub>0.375</sub>Sn<sub>0.625</sub> alloy for substituting Sb atoms and Bi atoms for Sn sties and Si sites, respectively, are calculated by first-principles calculations. The influence on electronic transport parameters is systematically analyzed by combining the calculated results of band structures and density of states. Corresponding component Sb and Bi atoms doped Mg<sub>2</sub>Si<sub>0.375</sub>Sn<sub>0.625</sub> alloys are prepared by rapid solidification method, and microstructures, Seebeck coefficients, and electrical conductivities of the alloys are measured. Combined with the predicted results by solving the Boltzmann transport equation, electronic transport performances are compared and analyzed. The results indicate that both Sn and Si sites are equally susceptible to Sb and Bi doping, but the Si sites are preferentially substituted due to their lower ∆<i>E</i><sub>f</sub> values. Doped Bi atoms provide a higher electron concentration, and Sb atoms offer higher carrier effective mass. Thus, the maximum <i>σ</i> value of the Mg<sub>2</sub>Si<sub>0.375</sub>Sn<sub>0.615</sub>Bi<sub>0.01</sub> alloy is 1620 S/cm. The maximum <i>S</i> value of the Mg<sub>2</sub>Si<sub>0.365</sub>Sn<sub>0.625</sub>Sb<sub>0.01</sub> alloy is –228 μV/K. Correspondingly, the highest <i>PF</i> value for this alloy is 4.49 mW/(m·K) at <i>T</i> = 800 K because of the dominant role of <i>S</i> values. Although its power factor is slightly lower, the Mg<sub>2</sub>Si<sub>0.375</sub>Sn<sub>0.615</sub>Sb<sub>0.01</sub> alloy is expected to exhibit lower lattice thermal conductivity due to the lattice shrinkage caused by substituting Sb sites for Sn sites. The optimal doping concentration of the Bi-doped alloy is lower than that of the Sb-doped alloy. These results are expected to provide a significant reference for optimizing the experimental performance of Mg<sub>2</sub>(Si, Sn)-based alloys.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.