Abstract

ABSTRACTThe 5-mm-thick AZ61 magnesium alloy was friction stir welded by using the specially designed bobbin tool with various rotation speeds. Defect-free welds were successfully obtained with rotation speed ranging from 550 to 600 rev min−1. Grain size in different regions of the joints varied depending on the rotation speed. The hardness value of the joint is uniform. The defective joint fractured in the weld nugget zone with the lowest tensile strength, while the fracture location of the defect-free joints changed to the heat affected zone. The impact energy of weld nugget zone is higher than that of the heat affected zone, and the impact energy of the two zones in defect-free joint both decreased with increasing rotation speed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.