The effects of varying the reverse pulse current duration (τ = 0 s, 1 s, 5 s, and 10 s) were evaluated on the composition, crystallinity, hardness, corrosion resistance, and tribological performance of nanolaminate Ni-W coatings deposited by pulsed reverse current electrodeposition. With the deposition conditions used in this study, it was found that a reverse current duration of τ = 1 s produced a coating that was both highly corrosion resistant and wear resistant.