Abstract

This study evaluated the influence of occlusal resin cement space on the fatigue performance of bonded-leucite crowns to a dentin-analogue material. Leucite anatomical crowns were adhesively cemented to dentin-like preparations having distinct occlusal cement space (50, 100 and 300 μm) (n = 18), and subjected to step-stress fatigue testing (150 N – 350 N; step-size: 25 N; 20,000 cycles/step; 20 Hz). Fatigue data (load and number of cycles for failure) were analyzed using Kaplan–Meier and Mantel–Cox (log-rank) tests (p <0.05). Fractographic analysis and occlusal internal space measurements were also performed. There was no significant difference for the distinct occlusal cement layer (50 μm: 289 N, 136,111 cycles; 100 μm: 285 N, 132,778 cycles; 300 μm: 246 N, 101,667 cycles). Occlusal internal space analysis showed a mean thickness of 120.4 (50 μm), 174.9 (100 μm) and 337.2 (300 μm). All failures were radial cracks originating at the ceramic-cement interface. Distinct occlusal cement spaces had no effect on the fatigue behavior of anatomical leucite crowns.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.