Abstract

To verify the influence of repeated microwave disinfections on the shear bond strength of two commercial types of teeth to acrylic resin, when the ridge lap surfaces were unmodified, bur abraded, bur grooved or etched by monomer. Eighty specimens (n = 10) were adhered to the tooth ridge lap surface, polymerised in a water bath at 74°C for 9 h. Microwaved specimens were individually immersed in 150 ml of water and submitted to five simulated disinfections in a microwave oven calibrated at 650 W for 3 min. Control specimens were not microwave treated. Shear bond strength tests were performed in an Instron machine with a cross-speed of 1 mm/min. The fracture load values were transformed into shear bond strength as a function of the bonding area (0.28 cm(2)). Data were submitted to ANOVA and Tukey's test (α = 0.05). Fractured areas were classified as adhesive, cohesive (resin or tooth) or mixed failures. Repeated microwave disinfections increased the shear strength of the tooth/resin bond. Mechanical retention in microwaved and non-microwaved procedures improved the shear bond strength. The different commercial types of teeth influenced shear bond strength values, with Biotone teeth showing the lower values.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.