Abstract
The study of the influence of the duration of preliminary high-energy ball milling on the features of the structural-phase state and the level of microhardness of consolidated Ni3Al samples obtained by the method of spark plasma sintering has been carried out. It was found that the inhomogeneous state of the precursor from the 3Ni-Al powder mixture in the case of preliminary ball milling of a short duration (1 min) is a cause of the formation of an inhomogeneous structural-phase state of the consolidated Ni3Al sample. An increase in the duration of high-energy ball milling provides a homogeneous phase composition, promotes the refinement of the grain structure and an increase in the microhardness values of the obtained Ni3Al samples. The main factors determining the processes of structural-phase transformation during the formation of Ni3Al under the conditions of spark plasma sintering, depending on the preliminary high-energy ball milling, are revealed. It is shown that grain boundary strengthening is the one of the effective mechanisms for increasing the strength of the material under study.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.