The effect of different pre-ageing treatments on the subsequent artificial ageing response of Al-Mg-Si(-Cu) alloys have been investigated using hardness, tensile and electrical conductivity testing. The microstructural evolution was characterised by differential scanning calorimetry (DSC) and 3-dimensional atom probe (3DAP) analysis. Pre-ageing treatments were carried out at 160-250°C for short times. Results show that the early stage artificial ageing response after 30 minutes at 170°C is strongly influenced by the pre-ageing and natural ageing conditions. A pre-ageing treatment performed for a short time at a high temperature and within a short delay after solution treatment and quenching was found to give a promising hardening response during subsequent artificial ageing. The mechanisms by which pre-ageing can reduce the detrimental effect of natural ageing on the artificial ageing response will be discussed in relation to the formation and distribution of clusters, GP zones and/or precipitates.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.