Abstract

Europium (Eu) doped nanostructure ZnO thin films are prepared by using spray pyrolysis technique. The ZnO:Eu thin films are deposited at a substrate temperature of 623K on glass substrates, using europium nitrate as a Eu source. The as-prepared ZnO:Eu films are annealed in air at 673K and 723K for 1h. The effect of post-annealing on the structural, electrical and optical properties of the films has been studied. XRD measurements show that all the films are nanocrystallized in the hexagonal wurtzite structure and exhibit a preferential orientation along (002) plane, the intensity of preferentially oriented (002) peak is apparently improved. The resistivity of annealed film is larger than the as-deposited. ZnO:Eu film annealing at 723K for 60min exhibits lowest resistivity of 3.62×10-4Ω cm. In addition, the ZnO:Eu film shows good optical transmittance of 94%.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.