In this research work, the effect of plastic synthetic aggregate in the production of lightweight concrete was studied. The plastic synthetic aggregate was used to replace 0-40% of coarse aggregates. A mix proportion of 1:1.8:3.7 with water cement ratio of 0.47 were used. Concrete cubes of 150mmx150mmx150mm of coarse aggregate/plastic synthetic aggregate were cast and cured at 3,7,28,60 and 90 days respectively. At the end of each hydration period, the three concrete cubes for each hydration period were crushed and their average compressive strength recorded. A total of ninety (90) concrete cubes were cast. The result of the compressive strength tests for 5-40% replacement of coarse aggregates with plastic synthetic aggregate ranges from 8.07-36.71N/mm2 as against 24.58-41.21N/mm2 for the control test. The workability for 5-40% replacement of coarse aggregates with plastic synthetic aggregate ranges from 12-61mm as against 8mm for the control test (0% replacement).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.