Abstract
Effect of pH and applied stress on hydrogen sulfide stress corrosion behavior of HSLA steel based on electrochemical noise analysis
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
https://doi.org/10.1007/s42243-023-00998-2
Copy DOIPublication Date: Jul 4, 2023 | |
Citations: 1 |
Effect of pH and applied stress on hydrogen sulfide stress corrosion behavior of HSLA steel based on electrochemical noise analysis