Abstract

Silicon-carbide particle (SiCp) preforms with particle sizes of 20, 50, 100 and 150μm were prepared by compression mold forming and heat treatment. A high resolution (~1.0μm) three-dimensional (3D) X-ray micro-computed tomography (X-ray μ-CT) combined with 3D pore-network models were used to study the effect of particle size on 3D characteristics and spatial structures of pores in the preforms. The results demonstrated that as the particle size increased, the gap expansion caused by burning of starch reduced. When the particle size increased from 20 to 100μm, the average areal porosity, homogeneity of pore distribution, connectivity, the numbers of small pores and throats, and average pore coordination number decreased; the average effective sizes of pores and throats increased. When the particle size further increased to 150μm, the large gaps were filled by small particles resulted from the broken coarse particles, which decreased the homogeneity and connectivity of pores. As a result, the pore-network analysis shows that the numbers of small pores and throats and average pore coordination number increased.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.