Abstract
Calcined diatomite was first investigated as matting agent for formulating high-performance coating. Jet milling and sieving or sedimentation methods were employed to obtain rational particle size distributions. It was found that the optimal size distribution of the particles with the diameters of D10 = 2.54 µm, D25 = 5.04 µm, D50 = 9.74 µm, D75 = 18.80 µm, and D90 = 31.66 µm showed the best extinction performance, with the gloss and extinction being 2.9 and 3.3 and 32.6% and 50.7% determined at incidence angles of 60° and 85°, respectively.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.