Extracting indium from water quenching slag, which contains poor indium, by two process of leaching, the effect of different oxidants and dosages on the leaching rate of indium in water quenching slag were studied. The leaching conditions: temperature 80 °C, leaching time 2 h, the liquid to solid ratio of neutral leaching 8︰1, the liquid to solid ratio of acid leaching 2︰1, initial concentration of sulfuric acid 500 g·L-1, adding different oxidants, the concentration was detected by crystal violet spectrophotometry. Test results showed that the leaching rate of indium was significantly improved by adding hydrogen peroxide and potassium permanganate. Compared with the effect of different oxidants, the effect of potassium permanganate was significantly higher than that of hydrogen peroxide on the leaching rate of indium.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.