API 5L X65 steel pipes with a 17.5mm wall thickness and 762mm in outer diameter were welded using an orbital automatic welding process. Flux Cored Arc Welding (FCAW) and Gas Tungsten Arc Welding (GTAW) consumables were utilized to evaluate automatic the welding process. Manual welds were deposited using GTAW with ER70S-G filler metal for the root pass and Shielded Metal Arc Welding (SMAW) with low hydrogen E9016-G electrode for the remaining passes. Charpy impact test, CTOD (Crack Tip Opening Test) test and micro-hardness test on the weld metal were carried out and the effects of weld metal composition and microstructure on the weld metal toughness were investigated. The filler metals that have superior fracture toughness were E80T1-K2 and E71T-1 of FCAW process and ER80S-G of GTAW process. The filler metals that have proper hardness were E80T1-K2 and E71T-1 of FCAW process.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.