Carbon-doping oxide materials (SiCOH films) with k of 2.62 are prepared by electron cyclotron resonance chemical vapor deposition (ECR-CVD) from the mixture of decamethylcyclopentasioxane (D5) and oxygen (O2). This paper investigates the effect of O2-doping on bonding configuration, dielectric property and leakage current of the SiCOH low dielectric constant films. The results show that the leakage current can be reduced obviously on the premise that dielectric constant k is kept at a lower value by small O2-doping amount. For the SiCOH film deposited under O2 flow of 3 cm3/min, the dielectric constant k as low as 2.62 and leakage current of 8.2×10-9 A/cm2 can be obtained.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.