Abstract

AbstractIn carrying out fatigue delamination propagation tests to assess the propagation rate versus a function of the energy release rate, the question arises as to the necessary number of cycles required to properly characterize the behavior. Tests were performed elsewhere on two different carbon/epoxy, multidirectional woven composite laminates containing a delamination using constant amplitude cycling by means of displacement control for various cycle ratios. The aim was to carry out the tests for cycles. Most specimens complied with this requirement. In this study, the fatigue data are analyzed including the first cycles, the first cycles, the first cycles, and cycles. It was seen that although the delamination length versus the cycle number could be quite similar between different cycle ranges, the Paris relation constants could be significantly different. It is suggested to carry out tests for as many cycles as possible.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.