Abstract
In the present study, the powder metallurgy route was used to successfully incorporate Ni-coated carbon nanotubes into Sn-Ag-Cu solder, to form a nanocomposite solder. Nanoindentation tests were performed on both composite and Sn-Ag-Cu solder samples to investigate their creep behaviour at room temperature. Characterization results revealed that with the addition of Ni-coated carbon nanotubes, the creep behaviour of composite solder improved significantly as compared to that of the unreinforced solder alloy. Moreover, increasing the maximum load from 20 mN to 100 mN increased the percentage reduction in creep strain rate from 4% to 28%, for the composite compared to its monolithic counterpart after 300 s of holding.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.