Abstract
Numerous methods have been used to produce high purity TiC. There is no previous study has been reported on the formation using single elemental powders of Titanium (Ti) and Carbon (C) with addition Nickel (Ni) by tungsten inert gas (TIG) weld method. In this work, TiC was synthesized via TIG method by arc melting elemental powder mixture of Ti and C at ~5 second (s) and 80 ampere (A). The effect Ni contents on TiC formation was investigated. The mixed raw material was ball milled for 24 hours followed by synthesis via TIG method. The arced samples were characterized by X-ray diffraction (XRD) and Scanning electron microscope (SEM). It was revealed, that small amount of Ni additive to the metal powder allows the production of dense and tough TiC.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.