In this project the morphology and microstructure of both conventional cast and melt spun of Al–20Si–9Fe–1.2Nb and Al–20Si–9Fe–1.2Nb–6Ni (at wt%) alloys were investigated. Therefore, in order to study the effect of added Ni on the morphology characteristics of the above-mentioned alloy, the resulting conventional cast and ribbons of Al–20Si–9Fe–1.2Nb and Al–20Si–9Fe–1.2Nb–6Ni alloys were synthesized and analysed using OM optical microscopy, X-ray diffraction, SEM scanning electron microscopy together with EDS energy dispersive spectroscopy. Observations exhibit that, XRD patterns of Al–Si–Fe–Nb and Al–Si–Fe–Nb–Ni ribbons revealed the peaks of only α-Al phase. Therefore, after adding of 6 wt% Ni, peaks of α-Al were shifted to the relatively lower angles with a very weak intensity. Furthermore, 6 wt% Ni addition causes homogeneously scattered colonies (size range 5 –25 μm) which contain fine spherical (primary Si and δ-Al4(FeNiNb)Si2 phases) particles in the α-Al dendrite of rapidly solidified Al–20Si–9Fe–1.2Nb alloy, the size of spherical particles were found to be in the range of 100 nm–1 μm.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call