Abstract

This article deals with the effect of adding nano CeO2 to act as a grain pinner/refiner to a known Cu-Al-Ni shape memory alloy. Elements were taken in a predefined ratio to prepare 300 g alloy per batch and melted in an induction furnace. Casting was followed by homogenization at 1173 K (900 °C) and rolling to make sheets of 0.5-mm thickness. Further, samples were characterized for microstructure using optical and electron microscope, hardness, and different phase studies by X-ray and transformation temperatures by differential scanning calorimetry. X-ray peak broadenings and changes were investigated to estimate the crystallite size, lattice strain, and phase changes due to different processing steps. A nearly uniform distribution of CeO2 and better martensitic structure were observed with increasing CeO2. The addition of CeO2 also shows a visible effect on the transformation temperature and phase formation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.