Abstract
Two multi-step (two-step and three-step) slow shot speeds were used in the vacuum die casting process of AZ91D magnesium alloy. The vacuum pressure variation in the die cavity before mold filling was monitored by using a pressure sensor. The microstructures of the produced castings were analyzed with optical microscope and image analysis software. The experimental results demonstrate that, the vacuum pressure in the die cavity at the beginning of mold filling is significantly reduced by using three-step slow shot speed, resulting in a low gas porosity level in the produced castings. At an appropriate multi-step slow shot speed, the dwell time of the liquid metal in the shot sleeve before mold filling can be reduced and the flow of the liquid metal in the shot sleeve at the later stage of the slow shot process can be restrained, which cause a low externally solidified crystal content in the produced castings.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Transactions of Nonferrous Metals Society of China
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.