AbstractThe effects of polymer molecular weight and temperature on the physical aging of poly(2,6‐dimethyl‐1,4‐phenylene oxide) (PPO) is examined. Gas permeability and refractive index were monitored during the aging process for PPO film samples at three aging temperatures below the glass transition temperature. Comparisons between the two samples of PPO that differ widely in molecular weight reveal an insignificant difference, which support the notion that above a critical molecular weight range there is little influence on aging rate. Increased temperature, over the limited range of 35–55 °C, results in higher aging rates for films made from both PPO materials. The rate of aging decreases strongly with increasing film thickness over the range examined, ∼0.4–25 μm. © 2007 Wiley Periodicals, Inc. J Polym Sci Part B: Polym Phys 45: 1390–1398, 2007

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.