Abstract

Ni/Cu co-doped in soda lime silicate (SLS) glasses were prepared by using normal melt quenchingtechnique at 1200oC for 3 h, and annealed at 500 oC for 3 h. The current composition was prepared based on theproposed ratio: (64.98-x)SiO2: 10CaO: 25Na2O: 0.02NiO: xCuO where x=0.0, 0.1, 0.2, 0.3, 0.4 and 0.5 mol%.The physical and optical properties of Ni/Cu co-doped in SLS glasses such as density, molar volume, refractiveindex and optical absorption were measured and discussed. The optical absorption spectrum of Ni/Cu co-dopedin SLS glasses measured at room temperature in the wavelength region 200–1100 nm were presented.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.