Abstract
The microstructures and mechanical properties of Mg–3Sn–0.1Ca–xMM (mischmetal, x = 0.3, 0.6, and 0.9 wt.%) alloys were investigated. Optical microscopy (OM), scanning electron microscopy (SEM) and X-ray diffraction spectroscopy (XRD) were used to characterize the microstructures and phase constitutions of the cast and rolled alloys. Room temperature tensile tests were conducted to obtain the mechanical properties and macro-textures to evaluate the texture weakening effect results of the MM. The results show that an abundance of second phase formed, confirmed as the (Ca,MM)MgSn phase, and the volume fraction increased with the increasing MM addition. The tensile yield strength of the as-cast alloys increased with the MM addition, but the elongation decreased. All of the rolled Mg–3Sn–0.1Ca–xMM alloys showed a strong basal texture, and only slightly decreased in intensity after annealing treatment due to the particle-stimulated nucleation of recrystallization. The as-annealed Mg–3Sn–0.1Ca–0.6MM alloys exhibited the highest tensile strengths of 266.5 ± 3.3 MPa and 136.1 ± 3.7 MPa, which are mainly ascribed to grain refinement strengthening, Orowan strengthening and texture strengthening.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.