Abstract
The (Y,Eu)2O3 precursor prepared by microwave with ultrasonic-assisted co-precipitation is superior to the one prepared by co-precipitation of conventional approach as well as co-precipitation assisted by microwave. The effect of preparation conditions on the morphology and particle size of (Y,Eu)2O3 precursor was completely investigated in this study. The ideal conditions were optimized as 0.25M Ln3+ ions concentration, 80°C reaction temperature, 90 minutes reaction time and 0 minute ageing time. Consequently, the (Y,Eu)2O3 precursor in the needle-like shape with average size of 0.25μm in diameter was obtained. The possible mechanism was also presented.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.