Abstract

PurposeThis paper aims to study the effect of Micro-arc oxidation (MAO) coating on stress corrosion and electrochemical behavior of aluminum alloy.Design/methodology/approachThe stress corrosion cracking behavior of 7050 aluminum alloy (AA7050) after MAO treatment was investigated in 3.5 Wt.% NaCl solution using the constant load ring. Electrochemical impedance spectroscopy (EIS) was used to evaluate the change of corrosion resistance of MAO specimens in 3.5 Wt.% NaCl solution, and appropriate equivalent circuits were established.FindingsThe results demonstrated that the MAO coating can improve the corrosion resistance of the AA7050 and avoid the reduction of mechanical properties caused by corrosion. In the initial stage of corrosion, the corrosion resistance of coated specimen decreased at first and then increased. In the middle and final stage of corrosion, the corrosion resistance of coated specimen decreased at first and then stabilized.Originality/valueThe long-term corrosion behavior of MAO specimens under stress was studied by constant load experiment and EIS. It has guiding significance for the application of MAO technology on aluminum alloy.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.