Abstract
Ferritic weld metal deposited with a self-shielded arc-welding process has intentional additions of aluminum, magnesium, titanium and zirconium. This results in a complex precipitation process that has been characterized with a combination of electron microscopy techniques. This work indicates that the formation of a spinel oxide is critical for the nucleation of nitrides of zirconium and titanium and prevents the agglomeration of aluminum rich oxides and the formation of large aluminum nitrides. High-resolution transmission electron microscopy has been used to characterize the core/shell structure of the precipitates with microalloying additions. Thermodynamic modeling of the precipitate formation during solidification is consistent with the microstructural observations. The evolution of precipitate formation is critical to limit large inclusions and improve weld metal toughness.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.