Abstract

In order to widen the application range of bioactive glass (BG), we prepared a bioactive glass as a composite matrix, strengthened by titania nanoparticles. The prepared composites had different amounts of both bioactive glass (49S) and titania in the weight percents of 1:3, 1:1 and 3:1, respectively. Bioactive glass sols (49S) in the system (SiO2CaOP2O5) were prepared following the solgel technique, then a solution of 2 wt% methylcellulose was added and stirred at room temperature. Precalcinated TiO2 nanopowder was dispersed in the sol and the prepared mixture was fired at 600 °C. The inhomogeneity problem in preparation of composite powder was overcome by using methylcellulose (MC) as a dispersant. The nanostructure composites were characterized using X-ray diffraction (XRD) and Fourier transforms infrared spectroscopy (FT-IR). The microstructure of the surfaces of the different composites was examined by scanning electron microanalysis (SEM) to verify the apatite formation. The results led us to the conclusion that the addition of MC reinforces the composites and increases the formation of an apatite layer in the presence of BG and titania content.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.