A series of lanthanum-doped ferric-based layered double hydroxides with the carbonate intercalation (Mg–Fe–La–LDHs) of different M2+/M3+ molar ratio and their corresponding calcined products were successfully synthesized and characterized. In order to understand the effect of metal compositions in these materials on their adsorption performances for arsenate, various factors such as solution pH, contact time and initial arsenate concentrations were investigated. The results showed that the maximum adsorption capacity for Mg–Fe–La–LDHs decreased with the increment of the M2+/M3+ molar ratio, but the reversed trend occurred for the calcined products of Mg–Fe–La–CLDHs. This difference is closely related to the different adsorption mechanisms for layered double hydroxides (LDHs) and calcined layered double hydroxide (CLDHs). It was found that the adsorption isotherms can be well described by the Langmuir equation, and the adsorption kinetics followed the pseudo-second-order kinetic model. The results suggested that the obtained Mg–Fe–La–LDHs with lower molar ratio of M2+/M3+ in the materials were more suitable for removal of arsenate, while their calcined products Mg–Fe–La–CLDHs with higher molar ratio of M2+/M3+ were efficient adsorbents for arsenate. When the M2+/M3+ molar ratio in the material was 4.38, the maximum adsorption capacity of CLDH-3 was as high as 47.4 mg g−1.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call