Li-containing La0.5Li0.5-xNaxTiO3 and La0.67Li0.2-yNayTi0.8Al0.2O3 solid solutions have been obtained by solid-state reaction route that involves chemical decomposition reactions. Complex impedance spectroscopy measurements demonstrate that the electrical properties in La0.5Li0.5-xNaxTiO3 and La0.67Li0.2-yNayTi0.8Al0.2O3 systems depend on different areas of the ceramic's grain and can be represented by the equivalent circuit consisting of two (when x = 0.5, y = 0.2) and three series-connected elements (0 ≤ x ≤ 0.4, 0 ≤ y ≤ 0.15). It has been shown that an increase in sodium concentration leads to a decrease in the ceramic's grain size for La0.5Li0.5-xNaxTiO3 and La0.67Li0.2-yNayTi0.8Al0.2O3 solid solutions. Substitution of lithium ions by sodium leads to an increase in the unit cell volume of the perovskite structure. It has been demonstrated that La0.67Li0.14Na0.06Ti0.8Al0.2O3 and La0.5Li0.4Na0.1TiO3 materials with low sodium concentration have the maximum value of dielectric constant.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.