Abstract
Abstract Cores with diameters of 144, 94, 69, and 46 mm and length-to-diameter (l/d) ratios of 0.75, 1, 1.25, 1.5, 1.75, and 2, were removed from beam specimens produced from eight different concrete mixtures. Compressive strength tests were conducted on a total of 1876 core specimens. Strength correction factors were determined for converting the strength of the cores with l/d ratios ranging from 1.75 to 0.75 to the strength of an equivalent standard specimen with a l/d ratio of 2. The effects of type and maximum size of aggregate and core diameter on these correction factors were examined. As it was expected, the correction factors gradually decreased with the decrease in l/d. The effect was found to be more pronounced for cores with a smaller diameter. The results also revealed that the effects of type and maximum size of the aggregate on correction factors were not significant. The proposed strength correction factors differ only slightly from those currently recommended in ASTM C 42/C 42M-04 [1] and they are very close to those proposed by Bartlett and MacGregor cited by Arioglu et al. [2–4].
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.