Abstract In this study, 6 mm thick plates of Al 6061 T6 alloy are joined by laser welding at four welding speeds (40 mm × s-1, 35 mm × s-1, 25 mm × s-1, and 20 mm × s-1). The welded joints are made using a 4000 W fiber laser welding machine. The effect of laser welding speed on the pores formed in the weld seam was investigated. In this manner, it was found that with a change in laser welding speed the amount of pores formed in the structure also changed. In addition, after the welding process, macroscopic examinations, tensile tests and the hardness tests were made. As a result of the experiments performed, it was determined that, the laser welding speed was highly effective for pore formation.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.