Abstract

ABSTRACT Objectives. To investigate the welding parameters on preparation of nickel-titanium (NiTi) orthodontic arch wires that can simultaneously level and retract anterior teeth by combining round wire to provide high flexibility with rectangular wire to provide high rigidity. The effects of voltage and number of welding points on tensile strength, transition temperature range (TTR), and penetration of laser beam were investigated. Materials and Methods. 15 mm segments of 0.018 in. round wire and 15 mm of 0.019 × 0.025 in. rectangular wire were laser welded under argon shielding. The laser voltage was varied between 170 and 210 V for one-point and two-point welding. Results. Incomplete welding was found only in one-point welding at low voltage while all others were joined completely. Mean maximum tensile force at fracture was increased with increasing voltage. One-point welding at 210 V gave rise to the highest force at fracture. Differential scanning calorimetry (DSC) of the welded joints showed a lack of the original TTR curve, indicating the loss of superelastic properties. Significance. Laser welding of NiTi orthodontic arch wires with different geometries provided acceptable strength for use in orthodontic treatment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.