Abstract

Over the past few decades, there has been much research on additive manufacturing in both the academic and the industrial spheres to overcome the limitations of conventional manufacturing methods, thereby enabling the production of complex designs for improved performance. To achieve this purpose, it is crucial to meticulously set suitable laser parameters within the context of microstructural characteristics, including type and fraction of defects, texture development, residual stress, and grain size, etc. In the present study, we focused on recrystallization behavior, a type of relaxation process for accumulated thermal stress during the L-PBF process, as a function of laser power applied on the L-PBF process. The laser power has significant effects on the amount of recrystallized grain, directly related to the recrystallization temperature. Within the range of laser power used in this study, a downward trend was observed in the recrystallization temperature as the laser power increased from 370 W to 390 W. This trend suggests that higher laser power leads to a faster cooling rate, influenced by the volume of melt pool as well as the amount of heat dissipation from the melt pool, resulting in higher thermal stress during the process.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.