This paper examines the effect of iron catalyst thickness on the straightness of growth of carbon nanotubes (CNTs) for microelectromechanical systems fabricated using the CNT-templated-microfabrication (CNT-M) process. SEM images of samples grown using various iron catalyst thicknesses show that both straight sidewalls and good edge definition are achieved using an iron thickness between 7 and 8 nm. Below this thickness, individual CNTs are well aligned, but the sidewalls of CNT forests formed into posts and long walls are not always straight. Above this thickness, the CNT forest sidewalls are relatively straight, but edge definition is poor, with significantly increased sidewall roughness. The proximity of a device or feature to other regions of iron catalyst also affects CNT growth. By using an iron catalyst thickness appropriate for straight growth, and by adding borders of iron around features or devices, a designer can greatly improve straightness of growth for CNT-MEMS.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.