Abstract
Magnetic properties and microstructures of sintered Nd-Fe-B magnets with different Nd-Cu powders addition (0, 2.7, 4.5, 6.2 and 8 wt%) and their corresponding diffused magnets using Tb-Cu alloys were studied systematically. The results showed that the enhancement of coercivity after diffusion was positively correlated with the intergranular phase proportion of the base substrates, and the relatively larger coercivity increments with 8.69 and 9.16 kOe were obtained at the addition of 6.2 and 8 wt% respectively, while the coercivity increments only reached 3.54 kOe and 4.00 kOe for the diffused magnets prepared by the substrates with 0 and 2.7 wt% Nd-Cu powders addition. The further microstructure analyses demonstrated that the higher coercivities were mainly attributed to the rather deeper diffusion depths of Tb elements, and the Nd-rich grain boundary phases in the base substrates were beneficial to construct the effective diffusion channels for subsequent diffusion process. Meanwhile, just due to the lack of efficient diffusion channels in the substrates with lower intergranular phase proportion, a large amount of Tb atoms accumulated on the interface between diffusion source and base magnet, forming a Tb-Fe transition layer and significantly deteriorating the utilization of heavy rare earths. This work supplemented insight and experimental foundation for the base substrate design in the preparation of diffused magnet with high performance.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.