Abstract

The effect of impact compression on age hardening behavior was examined for Meso20 and 6061 aluminum alloys using a single stage gun. The hardness of Meso20 and 6061 aluminum alloy applied with an impact compression (about 5.0GPa) after the solution treatment increased with the aging time. The cluster of point defects like stacking fault tetrahedral (SFT) was observed in the 6061 aluminum alloys with the impact compression (5.3GPa) after the solution treatment. Even after the impact compression, distribution of the aging precipitates was clearly identified.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.