Aging was carried out by introducing the materials into a climatic chamber under appropriate conditions of temperature, humidity and time. The materials are made of two types of weaving (2/2 Twill, 8H Satin) glass fibre, and (8H Satin) carbon fibre. The matrix was polyetherimide(PEI). In order to characterize the interlaminar fracture a mechanical test was carried out using the mode I Double Cantilever Beam (DCB) and mode II End Notched Fixed (ENF) tests. The analysis consists of knowing the different failure mechanisms which have generated the hygrothermal aging.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.