Abstract

Hybrid ratio effect on flexural properties of sugar palm/E-glass fiber hybrid-reinforced polyester composites has been investigated. Before being embedded, the sugar palm fiber was taken off from its original mesh, washed, alkali-treated, and chopped into ~10 mm long. The specimens were cut from composite plates having different hybrid ratios, fabricated using cold pressed technique. The total fiber volume fraction was kept at ~0.21, where four hybrid ratios, and two span-to-depth ratios were used. The E-glass was arranged unidirectionally and placed right on the surface of a bottom mold and wetted using the matrix, and the SPF was then evenly poured on the wet E-glass arrangement in randomly oriented pattern. Specimen preparation and testing were carried out according to the ASTM D790 standard, where the E-glass sides were placed in tension sides of the beams. It was found that flexural strength, and strain at maximum stress significantly increase with the increase of hybrid ratio.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.