Abstract

This study examined the effect of high irradiance and short exposure times on the depth of cure of six resin-based composites (RBCs). Bluephase PowerCure and the Valo X light-curing units (LCUs) were used to photocure bulk-fill RBCs for their recommended exposure times: Admira Fusion x-tra (AFX/20s), Aura Bulk Fill (ABF/20s), Filtek One Bulk Fill (FOB/20s), Opus Bulk Fill APS (OBF/30s), Tetric EvoCeram Bulk Fill (TEC/10s) and Tetric PowerFill (TPF/10s). In addition, all bulk-fill RBCs were tested for depth of cure with one short 3 s exposure time from the Bluephase PowerCure or the Valo X in the Xtra Power mode. The RBCs (n=10 per RBC) were inserted into a 4mm diameter metal mold and covered by a polyester strip before being photocured. After 24h of storage, uncured RBC was scraped away to determine the depth of cure of the RBCs. None of the RBCs achieved a 4mm depth of cure. The depth of cure of TEC and TPF was unaffected by the exposure times (recommended or short) when using the Valo X. The depth of cure of AFX/20s, AFX/Xtra Power, ABF/Xtra Power, FOB/Xtra Power, and OBF/30s RBCs was greater when using Valo X compared to the Bluephase PowerCure. It was concluded that short exposure times can reduce depth of cure and should only be used for some RBCs.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call