Fe-6.5wt.%Si alloy is an excellent soft magnetic material. Due to the appearance of ordering structures, the alloy shows poor ambient temperature ductility, and can only be cold rolled by specific rolling process. The rolling process with heat treatment is complex and time consuming. Meanwhile, high-energy electropulsing shows electroplastic effect. Heat treatment effect of the high-density electropulsing on microstructure and mechanical properties were investigated. The hot rolled sheet with 1 mm in thickness could be uniformly recrystallized in 33 s at 690 oC by appropriate high density pulses and the ductility was improved in comparison to the conventional heat treatment in a furnace. After the electropulsing treatment, the hot rolled sheet could be warm rolled by 50% reduction of the thickness after one pass without edge crack.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.