Abstract

Duplex stainless steel, consisting of ferrite and austenite, has good corrosion resistance and is often used in harsh marine environments. In this paper, welding on SAF2507 duplex stainless steel with 5 mm thickness was finished by laser beam welding (LBW) and gas tungsten arc welding (GTAW). The post-weld solid solution treatment was also conducted at temperature of [Formula: see text]C followed with cooling by water after 1 h. The results showed that both LBW and GTAW could produce well-produced welds. The microstructures of the welds were composed of ferrite and austenite phases. After solid solution treatment at [Formula: see text]C, the two-phase structure of LBW joint became uniform, while [Formula: see text] phase was produced in GTAW joint. The impact test of welded joints at room-temperature was carried out. After solid solution treatment at [Formula: see text]C, the impact toughness of LBW joints obviously increased, but the impact toughness of GTAW joint decreased with the fracture morphology of brittle mode. The electrochemical experiments on the welded joints showed that the pitting corrosion resistance of LBW joints improved after solid solution treatment, while the pitting corrosion resistance of GTAW joints decreased.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.